An FCC iron-carbon alloy initially containing 0.20 wt% C is
An FCC iron-carbon alloy initially containing 0.20 wt% C is
An FCC iron-carbon alloy initially containing 0.20 wt% C is carburized at an elevated temperature and in an atmosphere wherein the surface carbon concentration is maintained at 1.0 wt%. If after 49.5 h the concentration of carbon is 0.35 wt% at a position 4.0 mm below the surface, determine the temperature at which the treatment was carried out.
Is this the question you were looking for? If so, place your order here to get started!